I had a pretty good morning. Went to Overtons but they were out of resin. Went next to AgriSupply in Garner and bought a gallon of resin. I'll try this out and cancel the resin from the eBay company in Ohio. Mixed up the old can of resin which had a little over half a gallon left. My first batch was a quart but it started hardening before I was finished. The next batch was half a quart. This went along better. Mixed another half quart for the second tray which was on the trailer. It's a lot easier with the tray on the saw horses. My back hurt from bending over to the panel on the trailer. I finished both panels with the remainder of the one gallon can. That makes it 3 panels per gallon of resin. The new gallon should get me through the next 2 panels with resin to spare although I will run out of tape before I'm done.
Dinner was stouffers French bread pizza. I ate too much this evening.

  |     |  